| Test series | (kPa) | Rubber type | Rubber content (%) | Cycle number at failure, | (MPa) |
| 1-R#1 | 50 | R#1 | 5 | 230 | 43 | 100 | 360 | 91 | 150 | 410 | 120 | 200 | 440 | 152 |
| 2-R#1 | 50 | R#1 | 10 | 200 | 35 | 100 | 309 | 70 | 150 | 370 | 103 | 200 | 408 | 120 |
| 3-R#1 | 50 | R#1 | 15 | 190 | 26 | 100 | 280 | 54 | 150 | 330 | 82 | 200 | 350 | 97 |
| 1-R#2 | 50 | R#2 | 5 | 280 | 46 | 100 | 515 | 102 | 150 | 708 | 163 | 200 | 740 | 185 |
| 2-R#2 | 50 | R#2 | 10 | 200 | 35 | 100 | 330 | 72 | 150 | 395 | 105 | 200 | 427 | 122 |
| 3-R#2 | 50 | R#2 | 15 | 140 | 25 | 100 | 230 | 60 | 150 | 300 | 85 | 200 | 314 | 108 |
| 1-R#3 | 50 | R#3 | 5 | 230 | 65 | 100 | 349 | 125 | 150 | 410 | 171 | 200 | 431 | 193 |
| 2-R#3 | 50 | R#3 | 10 | 160 | 51 | 100 | 300 | 110 | 150 | 361 | 167 | 200 | 391 | 185 |
| 3-R#3 | 50 | R#3 | 15 | 117 | 25 | 100 | 256 | 62 | 150 | 303 | 90 | 200 | 421 | 105 |
| Control | 50 | ā | ā | 280 | 65 | 100 | 411 | 122 | 150 | 470 | 174 | 200 | 498 | 202 |
|
|