Centerline and weight of the sample.
| Parameter | Number | 1 | 2 | 3 | 4 |
| WW (mm) | 90 | 90 | 90 | 90 | CT (mm) | 2.0 | 2.0 | 1.8 | 1.8 | FW (mm) | 65.0 | 60.0 | 72.0 | 72.5 | OS (mm) | 50 | 50 | 52 | 45 | CL (mm) | 400 | 400 | 400 | 400 | RHA (%) | 11.53 | 10.92 | 12.46 | 12.96 | BN | 12 | 20 | 12 | 12 | RAN | 4 | 4 | 4 | 4 | RN | 1 | 3 | 1 | 1 | UCL (N) | 136849.52 | 139997.03 | 134796.78 | 133987.94 | Fabrication cost | Low | High | Low | Low |
|
|