Research Article
Effects of Shrinkage-Compensation on Mechanical Properties and Repair Performance of Strain-Hardening Cement Composite Materials
Table 5
Tensile and flexural properties of SHCC and Ex-SHCC mixtures.
| Mixture ID | First-crack strength (MPa) | Tensile strength (MPa) | Strain at tensile strength (%) | Flexural strength (MPa) | Deflection at flexural strength (mm) |
| SHCC30 | 1.22 (±0.18) | 4.49 (±0.42) | 1.86 (±0.20) | 11.13 (±1.17) | 2.32 (±0.25) | SHCC60 | 1.77 (±0.46) | 6.27 (±0.38) | 3.49 (±0.89) | 12.71 (±1.27) | 1.16 (±0.02) | Ex-SHCC30 | 1.20 (±0.10) | 4.54 (±0.51) | 0.52 (±0.18) | 14.38 (±0.54) | 3.44 (±0.35) | Ex-SHCC60 | 2.57 (±0.35) | 6.60 (±0.36) | 2.29 (±0.44) | 16.21 (±1.77) | 1.78 (±0.36) |
|
|