Pavement life extension (years).
| Maintenance treatment | Pavement life extension for TI > 6 | Treatment life for TI < 6 | Good | Fair | Poor | Good | Fair | Poor | Cracks < 5% | 5% < cracks < 20% | Cracks > 20% | Cracks < 5% | 5% < cracks < 20% | Cracks > 20% |
| HMA crack sealing | 2.4 | 1 | N | 7 | 5 | N | Fog seals | 0.1 | N | N | 2 | N | N | Slurry seals | 2.3 | 0.7 | N | 9 | 5 | 3 | Microsurfacing | 1.8 | 0.5 | N | 10 | 6.5 | 3 | PME (polymer-modified emulsion) chip seals | 1.8 | 0.5 | N | 10 | 6.5 | 3 | PMA (polymer-modified asphalt) chip seals | 1.8 | 0.5 | N | 10 | 7.5 | 5 | AR (asphalt rubber) chip seals | 3.8 | 2.8 | 0.7 | 10 | 7.5 | 5 |
|
|