Research Article
The Use of Waste Maroon Marble Powder and Iron Oxide Pigment in the Production of Coloured Self-Compacting Concrete
Table 5
UPV and density of the SCC series.
| Mixtures | UPV (m/s) | Density (kg/m3) | 3 days | 7 days | 28 days | 28 days |
| M1 | 4065 | 4385 | 4736 | 2.39 | M2 | 4098 | 4219 | 4557 | 2.38 | M3 | 4201 | 4237 | 4575 | 2.40 | M4 | 4184 | 4347 | 4694 | 2.38 | M5 | 4048 | 4201 | 4537 | 2.41 | M6 | 3891 | 4016 | 4337 | 2.40 | M7 | 3787 | 4098 | 4425 | 2.41 | M8 | 3558 | 4065 | 4390 | 2.39 | M9 | 3448 | 3891 | 4202 | 2.38 | M10 | 3184 | 3717 | 4014 | 2.40 |
|
|