Research Article
Effect of Sulphate and Chloride Ingress on Selected Cements Mortar Prisms Immersed in Seawater and Leather Industry Effluent
Table 6
Dapp and r2 values after exposure to SW for SO42−.
| Cement type | w/c | Dapp (×10−11 m2/s) | r2 | Cs |
| A | 0.5 | 1.065 | 0.945 | 1070 | 0.6 | 1.222 | 0.939 | 1050 | 0.65 | 7.821 | 0.936 | 1070 | 0.7 | 8.148 | 0.955 | 1590 | B | 0.5 | 1.061 | 0.955 | 1200 | 0.6 | 1.569 | 0.939 | 1400 | 0.65 | 9.810 | 0.942 | 1500 | 0.7 | 7.821 | 0.945 | 1600 | C | 0.5 | 1.065 | 0.939 | 1200 | 0.6 | 1.223 | 0.936 | 1300 | 0.65 | 1.569 | 0.933 | 1300 | 0.7 | 1.569 | 0.933 | 1200 |
|
|