Research Article

Experimental Study on Bond Performance and Damage Detection of Corroded Reinforced Concrete Specimens

Table 5

The expression of the ultimate slip and the corresponding parameter.

Equation corrosion rateEquationEquation stirrup ratio
asbsCover thicknessasbsasbs

-35-0−18.698.8C0-c/d-02.582.12C0-35-ρsv126.296.54
-35-150−16.869.53C0-c/d-1504.441.66C0-45-ρsv130.217.41
-35-100−21.6711.19C0-c/d-1006.61−0.83C0-55-ρsv242.58.42
-45-0−15.599.32C7-c/d-02.582.12C7-35-ρsv101.055.11
-45-150−22.0211.07C7-c/d-1505.292.97C7-45-ρsv125.955.37
-45-100−16.4412.02C7-c/d-1005.89−1.93C7-55-ρsv277.93.87
-55-0−53.615.23C15-c/d-01.733.4C15-35-ρsv93.254.62
-55-150−23.6213.59C15-c/d-1503.380.89C15-45-ρsv133.394.58
-55-100−28.8817.72C15-c/d-1005.52−1.77C15-55-ρsv281.542.82