The relation between deflections and strain and fatigue loading times for steel-plate-reinforced plate (corroded by carbonization) under the 200 kN load.

Fatigue cycles (104)Y-5 (με)Y-1 (με)W-1/2 (mm)

0254.5−360.71.09
50274.1−375.91.13
100286.9−390.91.40
150291.3−410.21.52
200308.2−440.31.88

Note. W-1/2: midspan deflection, Y-1: compressive strain at the top of the midspan, and Y-5: tension strain at the bottom of the midspan.