Research Article
Study on Fatigue Characteristics of Carbonation Erosion Prestressed Hollow Slabs in Whole Life Cycle
Table 16
Dynamic displacement growth rate of test plates under 2 million fatigue load cycles.
| ||||||||||||||||||||||||||||||||||||||||
Note. The dynamic displacement data under the 2 million fatigue cycle test of the uneroded test plate are set as 1. |