Study on Fatigue Characteristics of Carbonation Erosion Prestressed Hollow Slabs in Whole Life Cycle

Table 5

Compressive strength of standard specimen under carbonization erosion.

Specimen size (mm)StrengthPrecarbonization strength (MPa)Strength (MPa) (carbonization depth of 5 mm)Strength (MPa) (carbonization depth of 10 mm)

100 × 100 × 100C5053.554.459.461.068.969.0
55.561.569.8
54.262.068.3