Distribution statistics of broken pieces after combined sample failure.

Sample numberSize (mm)Total quality (g)Fractal dimensionAverage valueDamage form
0∼2.52.5∼55∼1010.0∼1515.0∼2020.0∼2525.0∼30

C-17.413.324.996.368.2220.330.0050.622.362.35
C-26.915.9411.478.7613.460.000.0046.542.31
C-37.022.566.795.3110.210.0022.2554.142.39
D-111.088.416.3612.4815.6128.380.0082.322.252.28
D-29.855.228.7610.5316.5427.550.0078.452.29
D-311.466.1211.9311.2214.580.0023.8479.152.31
E-114.836.9013.389.5410.2618.3236.51109.742.182.17
E-29.055.796.938.7411.61.0.0054.9697.082.23
E-37.0411.2810.537.574.3619.0129.6690.452.11