Chemical composition of MK samples used in past research studies.
| Research study | Oxides (%) | CaO | SiO2 | Al2O3 | Fe2O3 | MgO | K2O | P2O5 | SO3 | Na2O | TiO2 | LOI |
| [16] | 0.03 | 57.37 | 38.63 | 0.77 | 0.07 | 0.49 | 0.61 | 0.15 | 0.39 | 0.40 | 1.04 | [18] | 0.09 | 51.6 | 41.3 | 4.64 | 0.16 | 0.62 | — | — | 0.01 | 0.83 | — | [19] | 0.78 | 52.68 | 36.34 | 2.14 | 0.16 | 0.62 | — | — | 0.26 | — | 0.98 | [20] | 0.05 | 51.2 | 45.3 | 0.6 | — | 0.16 | — | — | 0.21 | — | 0.51 | [21] | 0.07 | 52.1 | 41 | 4.32 | 0.19 | 0.63 | — | — | 0.26 | 0.81 | 0.6 | [22] | 2.4 | 56 | 37 | 2.4 | 0.3 | 1 | — | — | 1 | 0.2 | — | [23] | — | 51.5 | 44.7 | 0.4 | — | — | — | — | — | 2.1 | — | [23] | — | 52.5 | 44.5 | 0.9 | — | — | — | — | — | 1.7 | — |
|
|