Mechanical Properties and Drying Shrinkage Investigation of Alkali-Activated Mortar Using Waste Glass Powder
Table 4
The curve-fitting parameters of drying shrinkage.
| Param | A0 | S1 | S2 | S3 | S4 | S5 | NS1 | NS2 | NS3 | NS4 | NS5 |
| b1 | 1.045 | 2.176 | 2.208 | 2.758 | 2.675 | 2.486 | 2.407 | 2.085 | 2.102 | 1.597 | 2.186 | b2 | 0.193 | 0.368 | 1.674 | 0.164 | 0.185 | 0.198 | 0.477 | 0.167 | 0.435 | 0.824 | 0.094 | b3 | 1.547 | 2.351 | 0.366 | 2.114 | 0.252 | 0.731 | 2.252 | 0.367 | 2.890 | 3.255 | 2.665 | b4 | 0.071 | 0.261 | 0.651 | 0.277 | 0.038 | 0.648 | 0.510 | 0.315 | 0.289 | 0.868 | 0.963 | m1 | 1.212 | 0.842 | 1.137 | 0.663 | 1.507 | 2.873 | 1.743 | 2.195 | 0.733 | 1.893 | 0.992 | m2 | 0.579 | 2.611 | 2.392 | 2.079 | 1.816 | 0.546 | 1.684 | 1.198 | 2.497 | 0.011 | 2.443 | m3 | 0.131 | 0.684 | 0.432 | 0.517 | 0.955 | 1.281 | 1.067 | 0.683 | 0.386 | 0.711 | 0.109 | m4 | 1.655 | 0.078 | 3.504 | 0.682 | 0.128 | 2.278 | 0.404 | 2.061 | 0.312 | 2.252 | 0.834 | m5 | 2.144 | 1.767 | 0.063 | 1.794 | 0.073 | 0.484 | 1.975 | 0.894 | 2.028 | 4.145 | 2.606 | m6 | 1.867 | 0.702 | 0.854 | 1.383 | 0.811 | 0.370 | 0.445 | 0.116 | 0.874 | 2.953 | 1.081 | | 0.178 | 0.683 | 0.473 | 0.316 | 0.269 | 0.046 | 0.202 | 0.448 | 0.918 | 0.115 | 0.548 | | 1.211 | 0.900 | 0.178 | 0.725 | 0.304 | 0.171 | 0.589 | 0.564 | 1.582 | 0.962 | 1.567 | | 0.245 | 1.200 | 1.272 | 0.457 | 1.304 | 1.590 | 1.218 | 0.659 | 0.911 | 0.839 | 0.502 |
|
|