Research Article
Minimizing Drying Shrinkage and Enhancing Impermeability of Foam Concrete Modified with Epoxy Resin
Table 3
Composition of FC specimens (kg/m3).
| Group no. | P.O. 42.5 | R·SAC42.5 | Silica fume | Fly ash | Slag | Water | Foam | Water reducing agent | EP | Epoxy curing agent |
| b0 | 2363.0 | 262.6 | 787.7 | 1050.2 | 262.5 | 898.0 | 66.8 | 70.9 | 0 | 0 | b1 | 2363.0 | 262.6 | 787.7 | 1050.2 | 262.5 | 898.0 | 66.8 | 70.9 | 65.6 | 21.9 | b2 | 2363.0 | 262.6 | 787.7 | 1050.2 | 262.5 | 898.0 | 66.8 | 70.9 | 78.8 | 26.3 | b3 | 2363.0 | 262.6 | 787.7 | 1050.2 | 262.5 | 898.0 | 66.8 | 70.9 | 91.9 | 30.6 | b4 | 2363.0 | 262.6 | 787.7 | 1050.2 | 262.5 | 898.0 | 66.8 | 70.9 | 105.0 | 35.0 | b5 | 2363.0 | 262.6 | 787.7 | 1050.2 | 262.5 | 898.0 | 66.8 | 70.9 | 118.2 | 39.4 |
|
|