Research Article

Sample Preparation Methods Affect Engineering Characteristic Tests of Municipal Solid Waste

Table 5

Shear strength variation of different samples under different vertical stress (×10−2 kPa2).

Vertical stress (kPa)50100150200300400

Wet method samples9.6469.2161.00144.57652.891496.01
Dry method samples40.9189.7589.3661.93312.57608.05