Research Article

Study on Preparation of Coal Gangue-Based Geopolymer Concrete and Mechanical Properties

Table 8

Compressive strength and flexural strength of each specimen cured at 60°C for 7 days.

NumbersG1G2G3G4G5G6G7C

Compressive strength (MPa)68.371.154.259.286.552.345.738.8
Flexural strength (MPa)4.724.264.194.035.523.943.543.33