Study on the Properties of an Ecotype Mortar with Rice Husks and Sisal Fibers
Table 6
Experimental results of anticrack performance and impermeability.
| Sample | Crack area/mm2 | Fracture reduction factor (%) | Maximum seepage pressure (MPa) |
| A0 | 3016.33 | ā | 0.19 | A1 | 0 | 100 | 0.36 | A2 | 38.68 | 98.72 | 0.33 | A3 | 53.36 | 98.23 | 0.35 | A4 | 116.81 | 96.13 | 0.23 | A5 | 122.36 | 95.94 | 0.22 | A6 | 66.61 | 97.79 | 0.24 | A7 | 179.85 | 94.04 | 0.17 | A8 | 132.14 | 95.62 | 0.21 | A9 | 158.34 | 94.75 | 0.19 |
|
|