Research Article
Fracture Performance of a Large-Stone Asphalt Mixture Based on a Monotonic Tensile Overlay Test
Table 3
Properties of asphalt material.
| Items | Units | Specification limits | Test results | Standard |
| Penetration (25°C, 5 s, 100 g) | 0.1 mm | 60∼80 | 70.2 | T 0604-2011 | Ductility (15°C, 5 cm/min) | cm | ≥100 | 150 | T 0605-2011 | Softening point | °C | ≥46 | 47.1 | T 0606-2011 | Density (15°C) | g/cm3 | | 1.028 | T 0603-2011 |
| RTFO at 163°C for 5 h | | | | | Quality change (%) | % | ±0.8 | -0.2035 | T 0609-2011 | Residual penetration ratio (%) | % | ≥61 | 70.5 | T 0604-2011 | Residual ductility (5°C) | cm | ≥6 | 8.6 | T 0606-2011 |
|
|