Research Article
Comparative Study on Clear Specimen Strength and Member Strength of Side-Pressure Laminated Bamboo
Table 3
Comparison of design strengths between side-pressure LB and structural materials.
| Materials | Design strength | Modulus of elasticity (MPa) | Tension (MPa) | Compression (MPa) | Bending (MPa) | Shear (MPa) |
| Larix spp. principis-Rupprechtii | 9.5 | 15 | 17 | 1.6 | 10000 | Larix spp. sibirica | 8.5 | 12 | 13 | 1.5 | 10000 | Pseudotsuga spp. LVL | 8.5 | 14.5 | 14.7 | 2.0 | 11000 | Pseudotsuga spp. PSL | 13.4 | 17.2 | 17.2 | 1.6 | 12400 | Side-pressure LB | 20.0 | 18.1 | 21.3 | 2.5 | 9200 |
|
|