Research Article

Fabrication and Electrical Characterization of Translucent Bi12TiO20 Ceramics

Figure 3

Plot output from the Rietveld refinement of the Bi12TiO20 ceramic sintered at 800°C for 3 hours. The dots represent the XRD data and the solid curve represents the calculated pattern. The difference plot is shown at the bottom of the graph.