Research Article

Characterization of WO3 Thin Films Grown on Silicon by HFMOD

Figure 3

X-ray diffractogram of WO3 films prepared on silicon substrates at 300 K and further annealed at different temperatures. The peak at ~ , related to the monoclinic phase, is indicated by an arrow.
591787.fig.003