Research Article

Full Aperture CO2 Laser Process to Improve Laser Damage Resistance of Fused Silica Optical Surface

Figure 5

Polariscope images (sample A was polished at the distance of 248 mm and 249 mm; sample B was polished at the distance of 249 mm and 250 mm).