Research Article

Metallurgical Aspects of Laser Surface Processing of PM Cr-V Ledeburitic Steel

Table 1

Results of retained austenite volume fraction measurements.

Depth below the surface (mm)0.10.20.30.40.50.60.7

Central region82 ± 281 ± 467 ± 763 ± 439 ± 516 ± 317 ± 3
Periphery61 ± 863 ± 657 ± 949 ± 430 ± 418 ± 315 ± 3