Research Article

Physicochemical and Microstructural Characterization of Injectable Load-Bearing Calcium Phosphate Scaffold

Figure 5

Representative SEM image showing cell attachment to the surface of CPC scaffold with cytoplasmic extensions (e) after culturing for 4, 11, and 21 days—images (a), (c), and (e), respectively. The other 3 images ((b), (d), and (f)) show the development of the calcium phosphate matrix over time.
149261.fig.005