Research Article

The Effects of Process Parameters on Evolutions of Thermodynamics and Microstructures for Composite Extrusion of Magnesium Alloy

Figure 6

Maximum temperatures for various initial extrusion temperatures during ES extrusion through ES die and at ram speeds of 2 mm/s with preheated temperature 400–420°C.
259594.fig.006