Research Article
Effect of Soil Burial on Tensile Properties of Polypropylene/Plasticized Cassava Starch Blends
Table 1
Percent decrease in tensile strength of PP/PCS after biodegradation.
| Starch contents (Wt.%) | % loss in tensile strength after 30 days | % loss in tensile strength after 60 days | % loss in tensile strength after 90 days |
| 0 | 0.66 | 1.44 | 2.05 | 10 | 11.24 | 16.88 | 25.77 | 20 | 13.09 | 14.71 | 29.43 | 30 | 12.45 | 18.96 | 31.16 | 40 | 15.45 | 16.65 | 30.14 | 50 | 16.17 | 20.88 | 40.66 |
|
|