Research Article
Biopolymer Doped with Titanium Dioxide Superhydrophobic Photocatalysis as Self-Clean Coating for Lightweight Composite
Table 3
Compressive strength of standard and LC concrete with different ratio of WLA to cement (wt/wt).
| Types of composite | Composite percentages (wt/wt) | Samples | Average compressive strength (MPa) | Density (kg/m3) |
| Lightweight | WLA | 55% | A | 19.35 | 1750 | 60% | B | 16.95 | 1683 | 65% | C | 15.88 | 1580 | 70% | D | 13.99 | 1468 |
| Standard composition | Commercial [8] | 17.20 | 1900 |
|
|