The Kinetics and Dry-Sliding Wear Properties of Boronized Gray Cast Iron
Figure 2
(a) Optical micrographs of the boronized at GCI 1223 K for 6 h, showing the hardness indentation variation with distance from surface to interior; (b) hardness values of the boronized GCI at 1223 K for 6 h; (c) hardness values of the quenched and tempered GCI.