Research Article

Parameters Controlling the Oxide Reduction during Sintering of Chromium Prealloyed Steel

Figure 9

Fracture surface of the fractured AstCrM + 0.5% C components with densities of (a) 6.5 and (b) 7.4 g/cm3 sintered at 1200°C for 30 min.
789373.fig.009a
(a)
789373.fig.009b
(b)