Research Article
Parameters Controlling the Oxide Reduction during Sintering of Chromium Prealloyed Steel
Table 9
Temperatures of the H2O, CO2, and CO peaks in relation to graphite addition; AstCrM + C material with the density of 6.8 g/cm3 sintered at 1200°C.
| Graphite addition (wt.%) | H2O peak | CO2 peak | CO peak | 1st (°C) | 2nd (°C) | 3rd (°C) | 1st (°C) | 1st (°C) | 2nd (°C) | 3rd (°C) | 4th (°C) |