Factors and levels used in the experiments.

FactorsExperimental condition levels
1 2 3

() Machined surface inclination angle (°) 100 110 120
() Axial depth of cut (mm) 0.1 0.25 0.5
() Spindle speed (min−1) 3200 3700 4200
() Feed rate (mm/min) 870 920 970