SEM micrographs of Al2124 + 1 wt.% CNTs spark plasma sintered at (a) 400°C, (b) 450°C, and (c) 500°C and Al2124 + 2 wt.% CNTs spark plasma sintered at (d) 400°C, (e) 450°C, and (f) 500°C.
535640.fig.006a
(a)
535640.fig.006b
(b)
535640.fig.006c
(c)
535640.fig.006d
(d)
535640.fig.006e
(e)
535640.fig.006f
(f)