Effects of Rolling Reduction and Strength of Composed Layers on Bond Strength of Pure Copper and Aluminium Alloy Clad Sheets Fabricated by Cold Roll Bonding
Figure 1
Schematic illustrations of (a) a specimen for the uniaxial tensile test and (b) a specimen for tensile shear test. (c) The magnified schematic illustration of (b) indicated as square dot lines in (b).