Research Article
Performance Evaluation of Stone Mastic Asphalt and Hot Mix Asphalt Mixtures Containing Recycled Concrete Aggregate
Table 8
ANOVA outcomes for HMA test results.
| Tests | SS | MS | | value |
| OAC | 17.387 | 1.449 | 5.883 | <0.01 | Stability | 159.723 | 13.31 | 122.565 | <0.01 | Flow | 58.083 | 4.84 | 90.755 | <0.01 | Density | 0.073 | 0.006 | 84.631 | <0.01 | VTM | 0.088 | 0.007 | 6.972 | <0.01 | VMA | 17.833 | 1.486 | 89.263 | <0.01 | VFA | 32.013 | 2.668 | 36.321 | <0.01 | Resilient modulus | 4502850 | 375237.5 | 144.752 | <0.01 | Rut depth | 134.489 | 11.207 | 87945.32 | <0.01 | Rut rate | 4.777 | 0.398 | 1587.373 | <0.01 |
|
|