Research Article

Utilization of Recycled Concrete Aggregates in Stone Mastic Asphalt Mixtures

Table 3

80/100 binder test results.

TestMethodValueStandard requirement

Penetration @ 25°C (0.1 mm)ASTM D584.784–95
Softening point (°C)ASTM D3647.247–49
Flash point (°C)ASTM D92289275–302
Fire point (°C)ASTM D92303>302
Viscosity at 135°C (Pa·s)ASTM D44020.254
Viscosity at 165°C (Pa·s)ASTM D44020.099
Specific gravityASTM D701.03