Research Article

Evaluation of Concrete Durability Performance with Sodium Silicate Impregnants

Figure 7

Result of measured potential in surface-impregnated concrete.
945297.fig.007a
(a) Potential (21 MPa, submerged condition)
945297.fig.007b
(b) Potential (21 MPa, tidal condition)
945297.fig.007c
(c) Potential (34 MPa, tidal condition)
945297.fig.007d
(d) Potential (21 MPa, atmospheric condition)