Research Article
The Influence of Aggregate Size and Binder Material on the Properties of Pervious Concrete
Table 7
The mix proportion of alkali-activated slag paste.
| L/Sg | 0.35 | 0.40 | 0.45 | Aggregate size | | B | | Volume percent of filled voids | | 80% | | Concentration of alkali activator | SiO2 = 106 g/L | | Na2O = 105 g/L | Amount of phosphoric acid | | 0.74 M | | Amount of slag (kg/m3) | 432 | 403 | 377 | Amount of alkali-activated solution (kg/m3) | 151 | 161 | 170 | Amount of aggregate (kg/m3) | 1684 | 1684 | 1684 |
|
|