Research Article
Investigation on Dynamic Recrystallization Behavior of Martensitic Stainless Steel
Table 1
The values of
and
under different deformation conditions.
| Temperature (°C) | Strain rate (s−1) | Zener-Hollomon parameter | (μm) |
| 900 | 0.001 | | 17 | 950 | 0.001 | | 25 | 1000 | 0.001 | | 30 | 1100 | 0.001 | | 48 | 1150 | 0.001 | | 75 | 1000 | 0.01 | | 24 | 1050 | 0.01 | | 31 | 1100 | 0.01 | | 37 | 1150 | 0.01 | | 59 |
|
|