Research Article

Fabrication of SERS Active Surface on Polyimide Sample by Excimer Laser Irradiation

Figure 4

20 000x magnification images on the fine structures of two SERS active surface areas fabricated at 40 (a) and 80 (b) mJ/cm2 fluences.
987286.fig.004a
(a)
987286.fig.004b
(b)