Review Article
Time Dependent Development of Aluminium Pitting Corrosion
Figure 13
Data and fitted trends for several 6xxx series aluminium alloys exposed to seawater immersion conditions at Esquimalt, BC, Canada. The changeover to mode 2 occurs at around 2-3 years of exposure. Data from Godard et al. [16].