Research Article
Resistance of Alkali-Activated Slag Concrete to Chloride-Induced Corrosion
Table 1
Oxide composition of GGBS and OPC.
| Binder type | Oxide composition (%) |
Ignition loss (%) |
Fineness (cm2/g) | CaO | SiO2 | Al2O3 | FeO | MgO | SO3 |
| OPC | 60.0 | 23.0 | 5.0 | 2.0 | 1.0 | 2.0 | 2.1 | 3120 | GGBS | 41.2 | 34.2 | 11.7 | 1.4 | 3.7 | 1.7 | 1.29 | 4290 |
|
|