Properties of the used polypropylene fibres.
| Density | Length | Cross section | Tensile strength | Modulus of elasticity | (g/cm3) | (mm) | (μm) | (MPa) | (MPa) |
| 0.91 | 12 | 35 × (250–600) | 340–500 | 8500–12500 |
|
|