Research Article

Preparation of Cementitious Material Using Smelting Slag and Tailings and the Solidification and Leaching of Pb2+

Figure 4

SEM photos of hydration products with different smelting slag content: (a) 55%; (b) 60%; (c) 65%.
(a)
(b)
(c)