Research Article
Preparation of Cementitious Material Using Smelting Slag and Tailings and the Solidification and Leaching of Pb2+
Table 3
The quasi-two-level dynamic model equation data.
| Sample | /mg·g−1 | /mg·g−1 | /g·(mg·min)−1 | |
| Tailing | 1.0234 | 1.0656 | 0.1130 | 0.9981 | Smelting slag | 1.1123 | 1.1446 | 0.1586 | 0.9996 | Cementitious materials | 0.6033 | 0.6169 | 0.3716 | 0.9998 |
|
|