Research Article
Effects of Seawater Corrosion and Freeze-Thaw Cycles on Mechanical Properties of Fatigue Damaged Reinforced Concrete Beams
Table 10
Residual capacity results of beams of B series.
| Number | Fatigue | Yield load | /mm | Ultimate load | /mm | Ductility factor | Yield modulus | load level | kN | kN | kN/mm |
| B1 | 0 | 52.12 | 2.67 | 62.05 | 5.27 | 6.34 | 19.52 | B2 | 0 | 49.81 | 2.58 | 58.5 | 4.89 | 4.24 | 19.31 | B3 | 0.2 | 43.39 | 2.42 | 53.44 | 5.43 | 4.87 | 17.95 | B4 | 0.2 | 45.25 | 2.20 | 58.1 | 5.38 | 5.69 | 20.62 | B5 | 0.3 | 39.66 | 2.50 | 51.74 | 6.88 | 5.61 | 15.89 | B6 | 0.3 | 40.75 | 2.49 | 48.71 | 4.54 | 5.61 | 16.34 |
|
|