Research Article
Development of a New Type of Alkali-Free Liquid Accelerator for Wet Shotcrete in Coal Mine and Its Engineering Application
Table 16
Testing results of compressive strength about sprayed concrete.
| Accelerator | Compressive strength of 28 days/MPa | Average strength/MPa | Compressive strength ratio of 28 days/% |
| Without adding accelerator | 38.2 39.9 | 37.7 38.0 | 35.8 37.7 | 37.9 | 100 |
| WT-1 type accelerator | 35.8 32.0 | 31.2 34.9 | 36.1 32.9 | 33.8 | 89.2 |
| GOR-I type accelerator | 26.7 30.1 | 27.4 28.8 | 26.5 27.5 | 27.8 | 73.5 |
|
|