Chemical compositions (% dry weight basis) of big bluestem after pretreatment.

ComponentScreen size (mm)
1248

Cellulose56.4 (1.2)a58.6 (0.9)a58.4 (0.5)a58.9 (0.6)a
Hemicellulose5.7 (0.6)b5.2 (0.3)b4.9 (0.7)b4.6 (0.2)b
Lignin28.6 (0.7)c28.0 (1.3)c29.8 (0.2)c29.6 (1.0)c