Selected physical and mechanical properties of 100Cr6 steel.
| Group of prosperities | Property | Unit | Value |
| Physical | Poisson number | | 0.30 | Specific heat | J·kg−1·K−1 | 475 | Density | kg·dm−3 | 7.81 | Thermal conductivity | W·m−1·K−1 | 46.6 | Electrical resistivity | Ω·mm2·m−1 | 0.22 | Electrical conductivity | S·mm2·m−1 | 4.55 |
| Mechanical | Thermal expansion | 10−6·K−1 | 11.4 | Modulus of elasticity | longitudinal GPa | 210 | tangential GPa | 80 | Bulk modulus | GPa | 140 | Poisson number | | 0.30 |
|
|