Research Article

Effect of Rubberized Bitumen Blending Methods on Permanent Deformation of SMA Rubberized Asphalt Mixtures

Table 4

Binder features.

Base bitumen (80/100 penetration)
Binder
designation
Rubber content (%)Blending processBlending apparatusBlending speed (rpm)Blending duration (hour)Blending temperature (°C)

Control (80/100 penetration bitumen)0N/AN/AN/AN/AN/A
TB (terminal blend binder)20Terminal blendHigh shear mixer10,0002210
CB (continuous blend binder)12Continuous blendPropeller mixer2001180

Not applicable.