Research Article

Influence of Deposition Condition on Y2O3 Coatings Produced by Pulsed Electrophoretic Deposition

Figure 3

Cross-sectional SEM images of films deposited at various Y2O3 concentrations in a suspension solution (0.5, 2.0, and 5.0 wt%), with bias voltage of 0.5 V and bias frequency of 1 kHz.
(a)
(b)
(c)